Table 11: Thermal properties values.
Thermal Conductivity (W/mK) |
Density (g/cm3) |
Specific Heat (J/g °C) |
Thermal Diffusivity (m2/s) |
|
Low-carbon steel |
54 |
7.85 |
0.49 |
1.40∙10-5 |
In-625 21 °C |
9.8 |
8.4 |
0.41 |
2.84∙10-6 |
In-625 760 °C |
20.8 |
8.4 |
0.59 |
4.20∙10-6 |
Tungsten Carbide |
110 |
15.63 |
0.3 |
2.34∙10-5 |
Stellite 1 |
14.85 |
8.69 |
0.423 |
4.04∙10-6 |
Colmonoy 6 21 °C |
11.74 |
8.1 |
0.4857 |
2.98∙10-6 |
Colmonoy 6 760 °C |
25.1 |
8.1 |
0.62 |
4.50∙10-6 |
CoNiCrAlY 25 °C |
5.5 |
7.992 |
0.473 |
1.45∙10-6 |